ASTM C1273 determines the tensile strength under uniaxial loading of monolithic advanced ceramics at ambient temperatures. This addresses, but is not restricted to, various suggested test specimen geometries as listed in the official standard. In addition, test specimen fabrication methods, testing modes (force, displacement, or strain control), testing rates (force rate, stress rate, displacement rate, or strain rate), allowable bending, and data collection and reporting procedures are addressed. Note that tensile strength as used in this test method refers to the tensile strength obtained under uniaxial loading.
Equipment required
By means of our ceramic testing expertise and modular product design, we will help find the testing solution that is right for you. Give one of our application engineers a call today for help with creating the best budget and testing plan according to ASTM C1273.
Recommended Test Machine
Force range of 5 kN to 600 kN (1,125 lbf to 135,000 lbf)
Adjustable test space
The most popular choice for static tension and compression tests
These dual column testers are available in both tabletop and floor standing models
Recommended Testing Accessories
Satisfies the requirements of ASTM C1273
Designed to grip cylindrical test specimens
Wedge design self-tightens to avoid specimen slippage